My Top Hat has a steel mast step (apparently not galvanised) and the mast is aluminium (as per usual). The mast step has on-going rusting problems, which I struggle with, with my bottle of rust fixer and metallic primers and paints, etc. A friend recently suggested that it could be corrosion (electrolysis?) between the two metals.
I'm interested to know what the mast steps of other Top Hats are made of?
We're preparing to slip her in coming weeks for anti-fouling and could do a mast and spar renovation while replacing the mast step - it would be good to know how others manage this.
Kind regards
Murray